Fully automatic rock point load bending creep test system
Instrument composition
This instrument is a column mounted structure, which consists of a base, gearbox, column, bracket, motor, controller, force sensing, software, etc. The power is transmitted to the gearbox through an electro-hydraulic servo, and the gearbox passes through a complete set of transmission mechanisms to drive the screw rod to drive the lower head to obtain the required upward speed, thus completing the test requirements.
Technical parameters
1. Point load test
1.1 Loading method: Automatic pressurization Large load: 50kN ± 10N Other specifications available for selection
1.2. Curvature radius of conical pressure plate at the ball end: 5mm; Top angle: 60 °
1.3. Built in deformation: 0~50mm; Accuracy: 0.001mm
1.4. Reaction frame Large load: 80KN
1.5. Point load intensity: displayed on the upper computer and recorded in the background
1.6 Controller loading displacement Large: 50mm
1.7. Loading speed: 0.001-50mm/min can be set arbitrarily; Loading speed: adjustable from 0.01 to 10KN
2. Uniaxial compression (cylinder method) test:
2.1 Test piece size: Φ 50mm x height 100mm; Φ 100mm × Height 100mm
2.2 Loading speed: 0.001-10mm/min; Can be set arbitrarily
3. Uniaxial compression (prism method) test:
3.1 Test piece size: side length 40mm; 80mm high;
3.2 Loading speed: 0.001-10mm/min; Can be set arbitrarily
4. Splitting test:
4.1 Test piece size: φ 100mm x height 40mm; 50mm in diameter and 40mm in height
4.2 Loading speed: 0.001-10mm/min; Can be set arbitrarily
5. Bending and tensile test:
5.1 Test piece size: 30mm × 30mm × 160mm;
5.2 Loading rate: 0.001-10mm/min; Can be set arbitrarily
description2